| Paper #116 | Improved Method of Testing Durability and Adhesion of Paints and Other Coatings |
| Hutchings I M, Shipway P H,, |
93NM033, Proc. ISATA Conference on New and Alternative Materials for the Automotive Industries, Aachen, 1993, 165-170.
|
| Paper #117 | Influence of Nozzle Roughness on Conditions in a Gas-Blast Erosion Rig |
| Shipway P H, Hutchings I M, |
Wear, 162-164, 1993, 148-158.
|
| Paper #121 | Measurement of Coating Durability by Solid Particle Erosion |
| Shipway P H, Hutchings I M, |
Surface Coatings and Technology, 71, 1995, 1-8.
|
| Paper #122 | The Influence of Nozzle Length on the Divergence of the Erodent Particle Stream in a Gas-Blast Erosion Rig |
| Stephenson A N J, Hutchings I M, |
Wear, 189, 1995, 66-69.
|
| Paper #123 | A Method for Optimizing the Particle Flux in Erosion Testing with a in a Gas-Blast Apparatus |
| Shipway P H, Hutchings I M, |
Wear, 174, 1994, 169-175.
|
| Paper #124 | The Abrasive and Erosive Wear of Polymeric Paint Films |
| Rutherford K L, Trezona R I, Ramamurthy A C, Hutchings I M, |
Wear 203-204, 1997, 325-334.
|
| Paper #127 | Novel Methods for Characterizing the Mechanical Durability of Automotive Paint Systems |
| Pickles M J, Trezona R I, Hutchings I M, Ramamurthy A C, Freese J W, |
SAE 980977, Presented at the SAE International Congress, Detroit, February 1998.
|
| Paper #129 | Erosive Wear of Fibrous Ceramic Components by Solid Particle Impact |
| Heuer V, Walter G, Hutchings I M, |
Paper No. 115, International Conference on Erosive and Abrasive Wear (ICEAW), Cambridge, September 1998.
|
| Paper #135 | Wear Testing Methods and Their Relevance to Industrial Wear Problems |
| Gee M G, Owen-Jones S, |
NPL (National Physical Laboratory) Report CMMT (A)92, December 1997.
|
| Paper #290 | Relationship between Microstructure and Erosive Wear Resistance of Plasma-sprayed Alumina Coatings. |
| Zhang X. S., Clyne T. W., Hutchings I. M., |
Surface Engineering 13 (5) (1997) 393-401,
|
| Paper #292 | Erosive Wear of Fibrous Ceramic Components by Solid Particle Impact. |
| Heuer V, Walter G., Hutchings I. M., |
Wear 225-229 (1999) 493-501,
|
| Paper #297 | A Full Factorial Investigation of the Erosion Durability of Automotive Clearcoats. |
| Trezona R. I., Pickles M J, Hutchings I. M., |
Tribology International 33 (2000) 559-571,
|
| Paper #298 | Solid Particle Erosive Wear Testing. |
| Hutchings I. M., |
ASM Handbook, vol. 8, ASM International, Materials Park, OH, USA, 2000, pp. 338-345,
|
| Paper #300 | Effect of Weathering on the Mechanical Durability of Automotive Clearcoats. |
| Trezona R. I., Hutchings I. M., Weakley A. P., |
Surface Coatings International, 83 (2000) 588-587,
|
| Paper #301 | Resistance of Paint Coatings to Multiple Solid Particle Impact: Effect of Coating Thickness and Substrate Material. |
| Trezona R. I., Hutchings I. M., |
Progress in Organic Coatings 41 (2001) 85-92,
|
| Paper #321 | Procedure for Gas Jet Erosion Testing. |
| Gee M G, Hutchings I M, Plint A G, |
NPL Report MATC(A)53, July 2001.
|
| Paper #352 | Critical Evaluation of Erosive Wear Testing |
| Hutchings I M, Gee M G, |
NPL Report MATC(D)02
|
| Paper #372 | Stepwise Erosion as a Method for Determining the Mechanisms of Wear in Gas Borne Particulate Erosion |
| Gee M G, Gee R H, McNaught I, |
Wear 255 (2003) 44 - 54
|